Analysis of Compression Failure in Multidirectional Wood Laminates
Student: VICTORY OKON TOM (Project, 2025)
Department of Mechanical Engineering
University of Uyo, Akwa Ibom State
Abstract
ABSTRACT This research analysis the compression failure in multidirectional wood laminates, vital in construction and engineering for their high strength-to-weight ratio. It begins with precise construction and engineering for their high strength-to-weight ratio. It begins with precise construction and engineering for their high strength-to-weight ratio. Plywood, solid wood, and adhesives are assembled with sample preparation for uniformity. Plywood, solid wood, and adhesives are assembled with sample preparation for uniformity. A compaction test ensures compliance with density meticulous bonding for robust interfaces. A compaction test ensures compliance with density meticulous bonding for robust interfaces. Density (ρ) is calculated using weight (W), area (A), and thickness (t), while compression ratio, determined by applied force (F) and original thickness (t), provides insights into compaction behavior. Various grain orientations are studied, affecting compressive strength, failure modes, and deformation patterns. Moisture content, crucial in compression failure, is addressed using the oven-dry method, revealing its influence on mechanical properties and behavior. Compression tests provide fundamental insights into compressive strength, deformation behavior, and failure modes. Solid wood exhibits significantly higher compression stress compared to standard laminate. Moisture content values are: solid wood (12.76%), standard laminate (12.41%), and plywood (8.16%). Among samples with different adhesives, three alternating design laminate wood with Para flex contact adhesive has the highest percentage (26.47%), while alternating design with VTRAC 401w Super Stick High-Tech Adhesive has the lowest (15.19%). The laminate wood with the highest initial weight density is three alternating design (6115.56 kg/m$^3$), and the lowest is Alternating design (4942.22 kg/m$^3$). For final weight density, three alternating design has the highest (4835.56 kg/m$^3$), and Alternating design the lowest (4390.37 kg/m$^3$). The "Alternating design" with adhesive Λ (657.78KN) demonstrates the highest compression stress, making it the preferred choice. This research provides a comprehensive understanding with implications for material selection, design, and manufacturing processes across applications.
Keywords
For the full publication, please contact the author directly at: victorytom25@gmail.com
Filters
Institutions
- Al-Hikmah University, Ilorin, Kwara State 2
- AL-ISTIQAMAH UNIVERSITY, SUMAILA, KANO STATE 1
- Al-Qalam University, Katsina, Katsina State 5
- Alex Ekwueme Federal University, Ndufu-Alike, Ebonyi State 87
- Alvan Ikoku College of Education, Imo State, (Affl To Univ of Nigera, Nsukka) 11
- Ambrose Alli University, Ekpoma, Edo State 478
- Anambra State College of Health Technology, Obosi, Anambra State 1
- Auchi Polytechnic, Auchi, Edo State 503
- Auchi Polytechnic, Auchi, Edo State. (affl To Nnamdi Azikiwe University, Awka) 3
- Audu Bako College of Agriculture Danbatta, Kano, Kano State 54